Inconel 718 is an age-hardenable Nickel-Chromium-Columbium (Niobium)-Molybdenum alloy with excellent corrosion resistant properties. It is a high strength alloy that is compatible in both high and low-temperature environments (-423 F - 1300 F) (253 C - 704 C). It exhibits excellent fatigue, creep, and rupture strength making it an ideal alloy for fabricating springs. It is a superior material choice to Inconel X750 at higher temperatures when material strength is a factor.
Wide Range of Operating Environments
The alloy retains 75% of its tensile strength up to 1300 F (704 C). Inconel 718 remains ductile in cryogenic environments and is suitable for low-temperature applications like compressed liquid natural gas or CO2 processing. It retains 85% of its ductility at temperatures down to -400 F (-240 C). 718 also performs better than Nimonic 90 at cryogenic temperatures. The material performs well in sour gas environments although there are other nickel alloys such as Inconel 625 and Inconel 725 that perform even better.
Inconel 718 Heat Treatment Specifications
Inconel 718 is also resistant to hydrogen embrittlement and stress corrosion cracking with HRc values as high as 40 when in the solution annealed and aged condition. To meet these requirements the NACE MR1075 specifications for heat treatment are followed. The material is typically solution annealed at 1850-1900 F (1010 - 1040 C) and precipitation hardened at 1450 F (780 C) up to 8 hrs.
High Fatigue & Material Strength
To meet high fatigue and material strength, heat treatment is conducted by solution annealing at 1700 - 1800 F (925 - 980 C) followed by a rapid cool and precipitation hardening at 1325 F (720 C) for 8 hrs. and furnace cooling to 1150 F (620 C) for 18 hours.
Features & Benefits of Inconel 718 Springs
Resists corrosion in most environments
High strength with tensile values as high as 230 Ksi (1590 MPa)
Easily fabricated into many spring and wire form elements
Endures high temperatures up to 1300 F (704 C)
Endures low temperatures down to -423 F (-272 C)
Form and Condition |
Tensile Strength |
Yield Strength (0.2% Offset) |
Elongation, % |
Hardness, Rockwell |
ksi |
Mpa |
Ksi |
Mpa |
Wire |
cold drawn |
Annealed |
80-120 |
550-830 |
35-75 |
240-520 |
45-20 |
- |
No. 1 Temper |
105-135 |
725-930 |
70-105 |
480-725 |
35-15 |
- |
Spring Temper |
170-220 |
1170-1520 |
150-210 |
1035-1450 |
5-2 |
- |
FAQ
Question: Are you a trading company or manufacturer?
Answer: We're manufacturer.
Question2: Could you help to design the product?
Answer: Yes, we have excellent R&D team, OEM/ODM orders are all welcome.
Question: Could you supply samples?
Answer: Yes, wecould supply samples according to your requirement.
Question: could we visit your factory?
Answer: Sure, factory visit is warmly welcome.